SVD Restoration Blog

What Causes Concrete Pitting and How Can You Prevent It?

Published 2026-08-05 · By Petro Romanovich Symoniv

If your driveway or garage floor is dotted with small pockmarks and shallow holes, you are looking at pitting, and understanding what causes concrete pitting is the first step to stopping it. In most Ontario homes, the culprits are de-icing salt, freeze-thaw cycles, and finishing errors made when the slab was poured. The good news from the GTA’s best concrete contractor is that pitting is largely preventable, and existing pitting can usually be repaired before it spreads.

Here is what actually causes those little craters, how to tell pitting apart from scaling, and how to protect your concrete going forward.

Macro view of concrete pitting with small pockmarks and exposed aggregate on a driveway surface
Pitting shows as small craters, often with a popped-out stone at the bottom.

What Concrete Pitting Actually Is (and How It Differs From Scaling)

Pitting, sometimes called popouts, shows up as small holes or pockmarks, usually a few millimetres to a couple of centimetres across, scattered over the surface. It is different from concrete scaling, which is the flaking or peeling of a thin layer across a broad area. Pitting is localized craters. Scaling is a sheet of surface coming off. They can share causes, but they are not the same defect, and telling them apart points you to the right fix.

Quick Take

Pitting is small, individual holes. Scaling is broad surface flaking. Both are usually driven by salt and freeze-thaw, but pitting often also traces back to how the slab was finished and cured when it was poured.

What Causes Concrete Pitting

Most pitting comes down to one or more of these:

Infographic showing the six main causes of concrete pitting
The main causes of concrete pitting at a glance.

Did You Know

A lot of pitting is decided before the concrete ever hardens. Finishing timing, air entrainment, and curing in the first 24 hours have more to do with a pit-free surface years later than almost anything you do afterward. That is why prevention starts at the source.

How to Prevent Pitting on New Concrete

If you are removing concrete or pouring or having concrete poured, these steps do the heavy lifting:

  1. Specify air-entrained concrete rated for freeze-thaw exposure for any exterior slab.
  2. Do not overwork the surface, and never finish while bleed water is sitting on top. Wait for it to evaporate.
  3. Cure properly. Keep the slab moist or covered for the first several days so the surface gains strength instead of drying out fast.
  4. Wait at least 28 days, then apply a quality penetrating sealer before the first winter.
  5. Keep de-icing salt off it entirely in the first winter, when the concrete is most vulnerable.

Pro Tip

New concrete is at its most fragile in its first winter. Use sand for traction instead of salt that first season, and get a penetrating sealer on before the cold arrives. That single winter of care prevents a surprising amount of long-term pitting.

De-icing salt on a concrete driveway, a leading cause of concrete pitting in freeze-thaw climates
Salt plus freeze-thaw is the top cause of pitting on Ontario driveways.

How to Protect Existing Concrete From Pitting

For concrete already in the ground, prevention is about keeping salt and water out:

Cause of Pitting How to Prevent It
De-icing salt and freeze-thaw Use sand or safe de-icer, seal the surface, improve drainage
Overworking or early finishing Correct finishing timing at the pour, wait out bleed water
Low or uneven air entrainment Specify freeze-thaw-rated air-entrained mix for exterior slabs
Reactive or soft aggregate Quality mix design and good curing; repair popouts as they appear
Chemical or acid exposure Keep fertilizers and acidic cleaners off; rinse spills promptly

This information is general guidance for Ontario conditions. SVD Restoration is not liable for outcomes from actions taken based on this article. For mix design, structural concerns, or a surface that is deteriorating, have the concrete assessed by a qualified professional.

Can Pitted Concrete Be Repaired?

Yes, in most cases. Light, shallow pitting can be filled and the surface protected. Widespread pitting is a good candidate for a resurfacing overlay, a thin new wearing layer bonded over the old slab that restores a smooth, sealable surface without a full tear-out. If the concrete is otherwise sound, resurfacing is usually far cheaper than replacement. Our guide on concrete resurfacing covers when it is the right call.

Frequently Asked Questions

Is concrete pitting a structural problem?+

Usually not on its own. Surface pitting is a durability and appearance issue in the top layer, not a sign the slab is failing structurally. That said, unsealed pits let more water and salt reach deeper into the concrete, and over years that can accelerate cracking and reinforcement corrosion. Address pitting early to keep a cosmetic problem from turning into a structural one, and have any cracking that comes with it assessed by a pro.

What is the difference between concrete pitting and scaling?+

Pitting is small, individual holes or pockmarks scattered across the surface, often with a popped-out stone at the bottom. Scaling is the flaking or peeling of a thin layer of the surface across a broader area. Both are commonly caused by de-icing salt and freeze-thaw, but scaling tends to point to a weak surface skin while pitting often involves finishing errors or reactive aggregate. Identifying which one you have guides the repair.

Can I prevent pitting on a new driveway?+

Largely, yes. The biggest levers are set at the pour: use freeze-thaw-rated air-entrained concrete, finish it correctly without sealing in bleed water, and cure it properly for the first several days. After that, keep de-icing salt off it through the first winter, use sand for traction, and apply a penetrating sealer once it has cured. Concrete cared for through its first winter pits far less over its lifetime.

Does sealing concrete stop pitting?+

Sealing greatly reduces the main driver of pitting by keeping salt and water out of the pores, which is where freeze-thaw damage begins. It is one of the most effective preventive steps for existing concrete. Sealing will not reverse pits that already exist, and it will not fix concrete that was poorly finished or lacks air entrainment, but on sound concrete a good penetrating sealer, reapplied on schedule, meaningfully slows pitting.

Should I repair or replace pitted concrete?+

It depends on how deep and widespread the pitting is and whether the slab is otherwise sound. Shallow, scattered pitting can be filled and sealed. Extensive pitting on a structurally solid slab is usually best handled with a resurfacing overlay, which restores a smooth surface at a fraction of the replacement cost. Replacement makes sense when the concrete is also badly cracked, heaving, or failing below the surface. A quick assessment settles it.

Pitting starts small, but every unsealed pit is a doorway for more salt and water. Catch it early, protect the surface, and resurface before it spreads. SVD Restoration repairs, resurfaces, and protects pitted concrete across the Greater Toronto Area so a few pockmarks do not turn into a full replacement.